Benchy Bow Curling

I'm attempting to increase my print speed with PLA+ on my Vcore 3.1 (Eva 3.0, 4048 fan with mosquito hotend and orbiter v2.5). Previously I've been able to print a benchy at about 34 min without any artifacts but I'm trying to achieve a 20 min benchy. I'm having issues with the bow curling up during printing. I'm also running into a problem with orca slicer limiting my flow rate lower than what I've set it to (changing to 0.2mm layer height fixes this). Things I've tried: reduce temp from 220 down to 215,210,205. Enablling and disabling overhang slow down at curled perimeters. - 2 perimeters, 10% infill, 3 bottom and top layers. 0.25mm layer height, 0.4mm width. - 500mm/s outer wall speed at 8500mm/s2. Overhand speeds are set to default. - 24mm3/s max flow. - Fan speed set to 100%, min layer time set to 0
No description
1 Reply
DocDoyle
DocDoyle5d ago
More cooling! Also check if the hotend fan is spooling up fast enough to actually cool when it is in the overhang area Mine doesnt but thats more slicer related If the fan is already at 100% try slowing down for the local overhangs

Did you find this page helpful?