Edge roughness on the first layer
Was it too high bed or nozzle temperature? Other?
#3do-🇪🇺 ASA black printed with V-Core 4 IDEX.
The suggested temperatures are:
- Nozzle: 220-250°C
- Heatbed: 100-110°C



2 Replies
What´s with the green stuff under the first layer? Is that tape or is that green filament that was printed with the other extruder?
It’s another filament (3DO PETG). I think my main issue was a wrong Z-Offset: I’ve tuned at 85°C for another filament but after tuning for 100°C I had a good result on another print