bridge problems
ive read what I can find but ive been unable to get this right so I could use some pro tips :P.
I am testing with Superslicer bridge flow tests, with ABS+ at 240C. Temp has been picked after a temp tower provided no dripping and good layer adhesion.
Bridge speed is at 100mm/s, 60% flow and 120% above bridges.
Its not hanging but I keep ending up with loose threads.
I tried:
- more / less flow
- 5 and 10C above and below current temp
- 60 mm/s
- more / less cooling (from none to 100%)
I think at 60mm/s and 50% flow it seems to be the best (tight lines) but still loose from the layer above it.
Any ideas what else I can try?