do i have too much cooling?
Did the EVA 3 dual 5015 upgrade on my minion recently. using a matte black pla around 240 and capped flow at 25 with my dragonfly and cht 0.6.
Almost perfect print just a few boogers.
Thoughts to what it might be?
7 Replies
correct-apricot•2y ago
whats your seam placement setting?
PLA at 240? probably don't need that much temp for PLA at that flow rate... what does a simple cylinder look like?
flat-fuchsiaOP•2y ago
@sherbs cyl looks good. i did a annex engineering test cube and had no issues, but that was a 18min print only. i could try to reprint at 230.
@seriosha seam pos was "aligned" in SS here's a pic from the slicer
flat-fuchsiaOP•2y ago
flat-fuchsiaOP•2y ago
the white parts are the seams so on all the edges basically
Fwiw, I print pla at 205C at 30mm flow rate (volcano nozzle)... Prob need a little warmer than that for standard length nozzle... Did you try a temp tower? Just wondering how you got to 240c?
flat-fuchsiaOP•2y ago
i was doing flow tests at 220 230 240 and 250
250 saw the most flow
but was super stinky
i have a cht 0.6
i will try a lower temp next time i print
for now the printer is apart to try and figure out sensorless homing